Date tehnice | |||
Densitate uscata | Kg/m3 lbs/cu.ft. | 225 14 | |
Rezistenta de rupere la rece (DS/EN ISO 8895_2006) | MPa lbs/cu.ft. | 2.8 406 | |
Modulul de ruptura (EN993-6: 1995) | MPa lbs/cu.ft. | 1.4 203 | |
Porozitate totala (EN 1094-4:1995) | % | 91 | |
Permeabilitate la gaze | nPm | 0.7 | |
Caldura specifica | kJ(kgxK) BTU/(lbs°F) | 0.84 0.2 | |
Coeficientul de dilatare termica reversibila (BS 1902: secon 5.3:1990) 20°C -750 °C | X10-6K-1 x10-6°F-1 | 5.5 3.1 | |
Rezistenta la tractiune (EN 1607) | kPa lb/in2 | 610 88.47 | |
Coeficientul de contractie la umiditate (EN 1604) 23 °C 90% RH – 48 h | % | 0.0 | |
Conductivitatea termica (EN 12667) λ 10 | 10°C 50°F | W/(mxK) BTU/(sq.ftxhx°F/in) | 0.061 0.49 |
Conductivitatea termica (ASTM C-182) | 200°C 392°F | W/(mxK) BTU/(sq.ftxhx°F/in) | 0.07 0.49 |
Analiza chimica Dioxid de siliciu Oxid de calciu | % SiO2 Al2O3 Fe2O3 MgO CaO Na2O K2O LOI | 47 0.2 0.1 0.4 42 0.1 0.1 9 | |
Test rezistenta la foc (EN 13501-1:2007 + A1:2009) | Clasa A1 | ||
Culoare | Gri |